Experimental and theoretical confirmation of the scaling exponent 2 in pyramidal load displacement data for depth sensing indentation.The physical foundation of FN = kh(3/2) for conical/pyramidal indentation loading curves.Penetration resistance: a new approach to the energetics of indentations.Penetration resistance and penetrability in pyramidal (nano)indentations.
P2860
description
2010 nî lūn-bûn
@nan
2010年の論文
@ja
2010年論文
@yue
2010年論文
@zh-hant
2010年論文
@zh-hk
2010年論文
@zh-mo
2010年論文
@zh-tw
2010年论文
@wuu
2010年论文
@zh
2010年论文
@zh-cn
name
The exponent 3/2 at pyramidal nanoindentations.
@en
The exponent 3/2 at pyramidal nanoindentations.
@nl
type
label
The exponent 3/2 at pyramidal nanoindentations.
@en
The exponent 3/2 at pyramidal nanoindentations.
@nl
prefLabel
The exponent 3/2 at pyramidal nanoindentations.
@en
The exponent 3/2 at pyramidal nanoindentations.
@nl
P2860
P356
P1433
P1476
The exponent 3/2 at pyramidal nanoindentations
@en
P2093
P2860
P304
P356
10.1002/SCA.20206
P577
2010-09-01T00:00:00Z