Platinum-bearing chromite layers are caused by pressure reduction during magma ascent.
about
Platinum-bearing chromite layers are caused by pressure reduction during magma ascent.
description
2018 nî lūn-bûn
@nan
2018年の論文
@ja
2018年学术文章
@wuu
2018年学术文章
@zh
2018年学术文章
@zh-cn
2018年学术文章
@zh-hans
2018年学术文章
@zh-my
2018年学术文章
@zh-sg
2018年學術文章
@yue
2018年學術文章
@zh-hant
name
Platinum-bearing chromite layers are caused by pressure reduction during magma ascent.
@en
Platinum-bearing chromite layers are caused by pressure reduction during magma ascent.
@nl
type
label
Platinum-bearing chromite layers are caused by pressure reduction during magma ascent.
@en
Platinum-bearing chromite layers are caused by pressure reduction during magma ascent.
@nl
prefLabel
Platinum-bearing chromite layers are caused by pressure reduction during magma ascent.
@en
Platinum-bearing chromite layers are caused by pressure reduction during magma ascent.
@nl
P2093
P2860
P1476
Platinum-bearing chromite layers are caused by pressure reduction during magma ascent
@en
P2093
Gelu Costin
Ria Mukherjee
Sofya Chistyakova
Tony Naldrett
P2860
P2888
P356
10.1038/S41467-017-02773-W
P407
P577
2018-01-31T00:00:00Z